Tabla zinc TiZn ( titan-zinc ).
Coala zinc TiZn ( titan-zinc ).
Foaie zinc TiZn ( titan-zinc ).
1x1000x2000mm.
- grosime tabla zinc TiZn titan-zinc
1mm = 0.1cm,
Format table titanzinc TiZn 1000x2000mm.
- latime tabla zinc TiZn titan-zinc 1000mm = 100cm = 1m,
- lungime tabla zinc Zn TiZn titan zinc
2000mm = 200cm = 2m
- aliaj tabla zinc TiZn
99.9% Zn minim 99.9%Zn.

In urma unei comenzi se pot aduce table zinc de grosimi, formate si suprafete diferite natur sau preoxidate ( prepatinate ).

Zinc sheet 1x1000x2000mm .
TiZn sheet thickness 1mm.
Titanzinc sheet dimensions 1000x2000mm.
Titan-zinc sheet width 1000mm.
Zn sheet length 2000mm.
Titan zinc sheet chemical composition 99.9% Zn.

On preorder we can offer different thicknesses and dimensions of zinc sheets.
The titanium zinc sheets are supplied in several types of treatment, they can be either as zinc sheets pre-weathered natural  with a light grey layer or pre-weathered with a dark grey layer or treated to look like copper, brass, bronze, gold, mirror stainless steel surface etc.. The top surface of the TiZn sheet is disrupted during a chemical process, which produces a "weathered" effect. The titan-zinc sheet is not damaged, only the natural transition from the gloss finish to the matt finish is accelerated because the natural process it would last for several years. The result of pre-weathering of the zinc sheet is a light or dark grey layer.

TiZn sheet enables an excellent processing and mecanical properties with if the titan-zinc sheets are processed at a temperature lower than 10 C. If the temperature is lower, the processed edges need to be heated. It is also necessary to ensure that the TiZn elements do not touch the normal steel or copper because in such cases the galvanic corrosion occurs in the presence of water. TiZn sheets should not be laid on bituminous strips or insufficiently dried impregnated lathing.
For other detailes please advice with the constructors.